公司網(wǎng)站:http://www.cqzhejia.com/b-xiangxuan/sell8618425/
產(chǎn)品參數(shù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 吸水率 | ASTM D-570 | 0.01> | % | |
線性模壓收縮率 | KPIC Method | 1.4-1.8 | % | ||
熔體流動(dòng)速率 | ASTM D-1238 | 45 | g/10min | ||
密度 | ASTM D-1505 | 0.91 | g/cm3 | ||
機(jī)械性能 | 抗張強(qiáng)度(屈服) | ASTM D-638 | 430 | ||
彎曲模量 | ASTM D-790 | 24,000 | |||
斷裂伸長率 | ASTM D-638 | 40 | % | ||
Izod沖擊強(qiáng)度(缺口) | ASTM D-256 | 4 | |||
洛氏硬度 | ASTM D-785 | 112 | R Scale | ||
電氣性能 | 體積電阻率 | ASTM D-257 | 1 | 1017ohm.H | |
耗散(損耗)因數(shù) | 1KHz | ASTM D-150 | 2 | ||
介電常數(shù) | 1KHz | ASTM D-150 | 2.3 | ||
介電強(qiáng)度 | Short Time | ASTM D-149 | 40 | KV/M | |
耐電弧性 | ASTM D-495 | 130 | sec. | ||
熱性能 | 比熱 | KPIC Method | 0.46 | ℃ | |
熱變形溫度 | ASTM D-648 | 140 | ℃ | ||
熱傳導(dǎo)性 | KPIC Method | 3 | |||
維卡軟化點(diǎn) | ASTM D-1525 | 156 | ℃ | ||
熔點(diǎn) | ASTM D-3418 | 169 | ℃ | ||
熱膨脹系數(shù)(線性) | ASTM D-696 | 8.5 | 10-5H/H℃ |